Day 28, 4 hours of work done. The preparation of staining boat Jake's boat. Spraying water on 220 grit sanded hull to raise the grain then sand down againg to 220. Using HVLP spray gun, spray on water based stain Once dry, lay out the fiber glass in preparation of epoxy application to hull.